carbon anode block (32) Online Manufacturer
Thermal Conductivity: 150-200 W/mK
Bulk Density: 1.55-1.75 G/cm3
Compressive Strength: 30-40 MPa
Electrical Resistivity: 8-10 μΩm
Bulk Density: 1.55-1.75 G/cm3
Coefficient Of Thermal Expansion: 2.0-2.5 X10-6/℃
Max. Working Temperature: 1800-2000℃
Bulk Density: 1.55-1.75 G/cm3
Bulk Density: 1.55-1.75 G/cm3
Porosity: 18-22%
Max. Working Temperature: 1800-2000℃
Ash Content: 0.3-0.5%
Coefficient Of Thermal Expansion: 2.0-2.5 X10-6/℃
Ash Content: 0.3-0.5%
Bulk Density: 1.55-1.75 G/cm3
Application: Used In Aluminum Electrolytic Cells
Bulk Density: 0.9-1.1 G/cm3
Apparent Density: 1.5-1.7 G/cm3
Thermal Conductivity: 120-150 W/mK
Porosity: 15-20%
Material: Graphite
Ash Content: 0.3-0.5%
Ash Content: 0.3-0.5%
Porosity: 15-20%
Electrical Resistivity: 8-10 μΩm
Material: Graphite
Shape: Square
Density: 1.6-1.8 G/cm3
Fixed Carbon Min: 98.5
Volatile Matter: 0.7% Max
Key Words: Recarburizer
Sample: Provide