thermal conductivity intermediate cathode carbon block (8) Online Manufacturer
Bulk Density: 1.55-1.75 G/cm3
Coefficient Of Thermal Expansion: 2.0-2.5 X10-6/℃
Ash Content: 0.3-0.5%
Porosity: 18-22%
Bulk Density: 1.55-1.75 G/cm3
Porosity: 18-22%
Bulk Density: 1.55-1.75 G/cm3
Application: Used In Aluminum Electrolytic Cells
Coefficient Of Thermal Expansion: 2.0-2.5 X10-6/℃
Ash Content: 0.3-0.5%
Max. Working Temperature: 1800-2000℃
Bulk Density: 1.55-1.75 G/cm3
Bulk Density: 1.55-1.75 G/cm3
Ash Content: 0.3-0.5%
Max. Working Temperature: 1800-2000℃
Flexural Strength: 10-14 MPa